Cat Café EU & US domestic

I've had Test-C 250 (tested at 260-270) crash in transit, but that's a low BB / BA formulation (Which is great from an absolutely zero PIP perspective, smooth as butter).

15 mins in a 170f oven gets it back into solution and doesn't recrash. Sealed, even with the shrink wrap it comes in still on the vial, no issue. A much more effective method than all the hot water/vent pin and hot plate techniques in my experience.
 
Rubber ok?

Overall yea crashing is just annoying in the end, not the biggest deal

Was definately my initial concern.

Sterilization temps for bromobutyl stopper is 249f and chlorobutyl 320f, for 20 minutes.

So at 170f we're below the rubber stopper limits, Also well below temps that would boil or harm any of the active ingredients, oil, BA, and BB.
 